Obtaining a balanced microstructure in the fusion zone on a super duplex stainless steel (SDSS) weld is a challenge. The present work reports the use of the Watts bath to correct the phase balance on laser-welded SDSS. Three different Watts bath times were used, and the microstructure of the weld bead was evaluated. The Watts bath was efficient to correct the undesirable unbalanced microstructure resulting from SDSS laser welding as the austenite percentage increased.

Addition of Nickel by the Watts Bath as a Way to Correct the Phase Balance on Nd:YAG Pulsed-Laser-Welded UNS S32750

da Cruz Junior E. J.
Methodology
;
Ventrella V. A.
Methodology
;
Settimi A. G.
Membro del Collaboration Group
;
Gennari C.
Conceptualization
;
Calliari I.
Methodology
;
Zambon A.
Methodology
2022

Abstract

Obtaining a balanced microstructure in the fusion zone on a super duplex stainless steel (SDSS) weld is a challenge. The present work reports the use of the Watts bath to correct the phase balance on laser-welded SDSS. Three different Watts bath times were used, and the microstructure of the weld bead was evaluated. The Watts bath was efficient to correct the undesirable unbalanced microstructure resulting from SDSS laser welding as the austenite percentage increased.
File in questo prodotto:
Non ci sono file associati a questo prodotto.
Pubblicazioni consigliate

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11577/3443451
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 4
  • ???jsp.display-item.citation.isi??? 3
social impact